Explosion-proof lam LED photodiffusion heat shrink tube is made of household materials, excellent transparency, good heat dissipation effect, insulation, protect glass from breaking.
1, White LED heat shrink tube can homogenize point light to area light.
2, light transmittance can be up to 85-93%, haze 95-99%, customizable.
3, ROHS compliant, mercury-free, UV-resistant, energy-saving and low carbon.
4, Applicable to t5, T6, T8, T10, t12 LED lights.
Shrinkage temperature 60℃
125℃ final shrink temperature
Working temperature: -55℃~125℃.
When cutting the tube, the length of the glass lamps is increased by 5mm, the glass lamps that have been washed with alcohol and dried are installed on the heat shrink tube for cutting. Place them in a tunnel oven at a constant temperature of 75-85℃ to shrink.
After 1-2 minutes, check whether the pipe shrinks. if not, let them decrease sequentially. if the temperature is a little high, the heat shrink tube will form crystalline and black spots. trim them with a craft knife after they are already cool, proceed to the next step to install if there is no problem.
| Product number | ID (mm) | size
(mm) |
lie flat (mm) | thickness | horizontal shrinkage coefficient | vertical shrinkage ratio |
| led pet 018
|
F18.0 | T5 (16±0.5) | 30.0±0.3 | 0.10±0.02 | 45±4 | 7-13 |
| LED pet 029 | F29.5 | T8 (26.0±0.5) | 46.8±0.3 | 0.10±0.02 | 45±4 | 7-13 |
| led pet 033
|
F33.0 | T10 (32±0.5) | 55 ± 0.3 | 0.10±0.02 | 45±4 | 7-13 |
| Standard color: white, other colors can be customized. | ||||||
| No | Project | property requirements | test method |
| 1 | external | white, no pollution, no pin hole, no irregular colors, no mechanical damage | visa |
| 2 | appearance (not melted material) | See “Disorder Definition Scheme” in Appendix 1. | cut the diffusion film into 10 mm
visual inspection under fluorescent lamp and comparison with “garbage measurement chart” |
| 3 | resistance | 2.0kv.ak × 60 sec,
don't destroy |
dielectric strength tester |
| 4 | heat resistance | Put the heat shrink tube into the oven, 160 ℃ × 15 min, without breaking,
no color fading |
high temperature oven test |
| 5 | resistance to | surface wear is not obvious | Dip 100mm in isopropanol for 60 + 10 seconds and brush lightly.
(do not contact with acetone, ethyl acetate, dichloromethane and other organic solvents). |
| 6 | raft | 1.3-1.4 (g/cm)3) | ASTMD 792 |
| 7 | stretching | >107(n/m2) | ASTMD 638 |
| 8 | elongation at break | >62.0% | ASTMD 638 |
| 9 | water absorbed | <2.0% | ASTMD 570 |
| 10 | dielectric strength | > 15 (kV/mm) | ASTMD 149 |
| 11 | surface resistivity | >107(Ohm) | ASTMD 257 |
| 12 | volumetric resistivity | >1014(Ommm) | ASTMD 257 |
| 13 | fire resistance | HB | UL 94 |
| 14 | light transmission | 89.0±3.0% | fixed standard lamp (glass tube does not experience the luminous flux of the sleeve, expansion of the sleeve)
Loose film test luminous flux b transmittance = B/a)
The transmittance of the same film tube changes to 2% when 2 and 60 hours are below 10,000 hours. (the product cannot be used above 90s, and the transmittance is reduced by 5% due to the crystallization of the material). |
| 15 | Temperature test results | 1, LED diffusion film has been practically illuminated for 8000 hours. The value and transmittance of the Petg diffusion membrane did not change. | |